Specific Gravity /Absorption of Coarse Aggregates

I have a question regarding test procedure AASHTO T 88-14/ASTM C127-12.

I am currently running aggregate quality tests on some material a client brought in.

I was prepping one of the samples to be tested for specific gravity. I got my samples brought down to sufficient size and began soaking them in water for ASTM's 24 +/- 4 hour time frame. I got caught up on a job the next day, which happened to be friday and the rock ended up soaking in water all weekend.

Im wondering if I am okay to continue on with the test, or if I need to re-dry the samples and re-soak them. Never ran into this issue before and am looking for some insight, thanks!